Case Study: Reinforced Welded Corners in Chromic Acid Tank Sealed Using SylWrap HD
After new corners were welded in place during the repair and reinforcement of a badly corroded chromic acid tank at a factory in Argentina, SylWrap HD Pipe Repair Bandage provided sealing security against any leaks in the welding. Patches were cut from the bandage and smoothed up the entire 1.5 metre length of each reinforced corner.
Case Study Overview
Site Chroming factory
Location Argentina
Repair Type Tank repair
Defect Reinforcement and sealing of corroded tank corners
Repair Products
SylWrap HD Pipe Repair Bandage
Case Study PDF

Case Study Details
The iron tank was at a chroming factory in Argentina. It held chromic acid and was used during the re-chroming process of piston parts for oil extraction pumps. It was 10 metres long, 1.5 deep and 1.5 metres wide.
After a long time in service, the tank was suffering from corrosion. The damage was particularly heavy in the corners. The factory decided to repair the chromic acid tank, which involved installing welded reinforcements to each inside corner.
Not wanting to risk the possibility of there being leaks in the welding which could cause a future escape of chromic acid, the factory used SylWrap HD Pipe Repair Bandage to provide additional sealing security to the corners of the tank.


The normal method of application for SylWrap HD is to activate the resin, then wrap around the pipe or structure requiring repair whilst the bandage cures to form a rock hard material.
Wrapping was obviously not possible to the inside of the tank. Instead, the factory unwound their SylWrap HD and cut it into patches, making sure not to contaminate the bandage with dirt or grime.
These patches of SylWrap HD were then activated and smoothed as tightly as possible up the entire 1.5 metre length of the welded reinforcement, creating a watertight seal between the weld and the existing frame of the tank.

SylWrap HD was applied to all four corners of the tank in this way. Within 10 minutes of application, it had completely set to encompass each welded corner and cover any gaps or holes which may have otherwise been left exposed.
The final stage of the tank repair saw an acid-resistant PVC covering added. Whilst SylWrap HD offers good resistance against chemicals including sulphuric acid (which is a stronger concentration than chromic acid), this additional step was taken with the aim of further protecting the entire tank from future corrosion and attack.
Products Used
SylWrap HD Bandage
Composite wrap used to encompass parts and surfaces which sets rock-hard for ultimate protection
Related Case Studies
Case Study: Leaking Dishwasher 50mm Plastic Pipe Repair in Golf Clubhouse Kitchen
Case Study: Bilge Pipe Leaking Through Corroded Welded Joint Repair On Board Superyacht
Case Study: Corroded 30-Metre Section of Sewer Force Main In Underground Vault Repair
Case Study: Emergency Live Leak Pipe Repair Keeps Heating on at Nursing Home
Case Study: Repair of Leaking & Corroded Shared Water Supply Pipe Connected to Eight Cottages
If you have an application you would like to enquire about, then please get in touch
Call: +44 (0)1444 831 459
Email: sales@sylmasta.com